This publication presents the main characteristics of the recently developed High Fluidity (HF) Alloy that is based on the traditional Zamak composition and the earlier developed copper-rich alloy marketed under the names of Superloy and GDSL.

Download »

Learn the latest about Zinc. Sign Up.

  • This field is for validation purposes and should be left unchanged.

Locations

United States

1000 Park Forty Plaza, Suite 130
Durham, NC 27713, U.S.A.
P: +1 919 361 4647
E: contact@zinc.org

Belgium

Avenue de Tervueren 168
Brussels, 1150, BELGIUM
P: +32 2 776 0070
E: contact@zinc.org

India

G-1 & G-5 Ground Floor
Plot No.9, Allied Bhawan
Madangir, New Delhi, 110062, INDIA
P: +91 99 1029 9297
E: rsharma@zinc.org

China

Distrii Kangding Center
2/F, No. 1018 Kangding Road, room 266
Jing'an, Shanghai, CHINA
P: +86 (21) 22876655
E: ahuang@zinc.org

Zinc College

June 12-16, 2022 Eurostars Palacio de Cristal Oviedo, Asturias, Spain

2022 Zinc Metal Roundtable

November 15-16, 2022

Asia Pacific Roundtable Zinc

September 13-15, 2022 New Hotel: The Westin Desaru Coast Resort Desaru Coast, Johor, Malaysia

Zinc Die Casting Conference - Europe

October 5-7, 2022 Rhein-Mosel-Halle Koblenz, Germany

2023 International Zinc Conference

February 26-March 1, 2023 The Westin Kierland Resort Scottsdale, Arizona, USA